Etap pou pwodwi tèmik chòk ki estab alumina kre esfè brik

Dec 04, 2024

Sèvi ak esfè alumina kre kòm granula ak ajoute kantite lajan ki apwopriye nan SiO2 ak silikate wòch nan matris la, alumina kre esfè brik ak bon estabilite chòk tèmik ak ba re tire liy chanjman chanjman yo te pwodwi.
The main component of ordinary alumina hollow sphere products is Al2O3 (over 98%), and the matrix is composed of α - Al2O3, which is the main raw material causing poor thermal stability of the products. Therefore, when determining the formula, alumina hollow spheres are still used as aggregates, and an appropriate amount of SiO2 is added to the matrix. During the firing process, a certain amount of mullite phase is formed in the matrix to replace corundum phase, thereby improving thermal shock stability. Add a certain amount of silicon wire stone to the matrix to reduce the rate of change in the re firing line of the product and ensure the external dimensions of the product. The use of chemical binders can have adverse effects on the high-temperature performance of products, so chemical binders are not used. From these aspects, the following four formulas have been designed, and the thermal shock stability of their products is in the order of>20 times,>20 fwa, 5 fwa, ak 1 tan.

 

 

 

 

 

 

 

Kontakte mwen: Imèl: {{1 }/sdwenping@163.com

Tel: 86-0533-4188518 / faks: 86-0533-4188518

Rose: +86-13275332819 (WeChat/WhatsApp nimewo)

 

You May Also Like
Voye rechèch