1, paramèt pèfòmans pwodwi
ATIK | INITE | FSC-300 | FSC-400 | FSC-220 | FSC-550 |
Tanperati travay | degre | 1000 | 1000 | 1000 | 1200 |
Dansite | Kg/m3 | 300±10 | 400±10 | 220±10 | 550±10 |
Fòs konpresyon | Mpa | Pi gran pase oswa egal a 1.5 | Pi gran pase oswa egal a 2.0 | Pi gran pase oswa egal a 0.33 | Pi gran pase oswa egal a 0.6 |
Lineyè kontraksyon 900 degre * 3h | % | Mwens pase oswa egal a 1.0 | Mwens pase oswa egal a 1.0 | 1000 degre * 3h Mwens pase oswa egal a 2.0 | 1100 degre * 3h Mwens pase oswa egal a 3.0 |
Konduktivite tèmik 900 degre | W/m.k | Mwens pase oswa egal a 0.11 | Mwens pase oswa egal a 0.13 | 700 degre Mwens pase oswa egal a 0.09 | 1100 degre Mwens pase oswa egal a 0.14 |
Aplikasyon prensipal yo | Elektwolitik endistri aliminyòm | Elektwolitik endistri aliminyòm | Endistri siman | Endistri siman |

2, Karakteristik Xonotlite Composite Board:
1) Ti konduktiviti tèmik, bon efè izolasyon chalè
2) Kontraksyon tanperati ki wo se ti ak gwosè se ki estab
3) ti dansite, pwa limyè, mwens kapasite chalè
4) pwopriyete ki estab fizik ak chimik, bon efè itilizasyon
3, Aplikasyon: li se sitou itilize pou kouch izolasyon tèmik nan endistri aliminyòm elektwolitik, endistri siman ak lòt endistri
4, konpayi nou an pwomèt kliyan yo: bay echanj teknik gratis ak sèvis ak kliyan, epi bay echantiyon yo bay kliyan gratis san okenn frè echantiyon.
5, Reyalizasyon pwodwi: Konpayi nou an te deja anbake 90 tòn nan Omàn.
Èske ou vle jwenn yon founisè pwofesyonèl Xonotlite Composite Board?
Ou vle jwenn yon founisè ki estab ak kredib?
Lè sa a, tanpri kontakte avèk nou
Kontakte mwen:
Imèl:wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / FAKS: 86-0533-4188518
Rose:+86-13275332819(wechat/whatsapp nimewo)
Baj popilè: Xonotlite Composite Board, Lachin, manifaktirè, founisè, faktori, itilizasyon, pwopriyete